A painter at the shop next door asked why I was prepping with 80 grit, and it stung but he was right
Honestly I had been blocking out filler with 80 grit on every job for close to a year because it cut fast and I figured the primer would hide it. This painter from the shop across the lot watched me sand a quarter panel for about 30 seconds and said, "you're scratching past your filler, that's why your prime keeps flashing." I switched to 180 for the final pass and started guide coating with a cheap dry powder, and the scratches stopped showing up under the sealer. Tbh it added maybe 15 minutes per panel but cut my rework way down, and I've been doing it that way since March. Has anyone else had a painter call out their grit and then changed their whole sanding step?