Tried a heat gun to pull a dent on a '14 Civic fender and the paint blistered in about 8 seconds
I'd heard guys swear by warming the panel first so the metal moves easier, but on this factory silver it just cooked the clear and left me sanding a spot the size of a coaster, so what temp or tool are you all actually using on factory paint?